Data for: Impact of residual stress on thermal damage accumulation, and Young's modulus of fiber-reinforced ultra-high temperature ceramics

Published: 19 October 2018| Version 1 | DOI: 10.17632/p7dnzkd984.1
Contributors:
Pietro Galizia,
,
,

Description

The relative dimensional change (ΔL/L0) versus temperature was measured up to 1300 °C under flowing argon with a 5 °C/min heating rate using a dilatometer Netzsch mod. DIL E 402 (Netzsch, Geraetebau, Germany), on 25 mm x 2.5 mm x 2 mm bars

Files

Categories

Dilatometry, Thermal Precipitation