FTIR Analysis for the carbon fiber composite (no coat)

Published: 1 August 2018| Version 1 | DOI: 10.17632/4n3cf9j6mt.1
Contributor:
Ibrahim Alarifi

Description

show the highest peak at 3744 to 3373 cm-1, which means that there was a presence of Hydroxyl groups and there was O-H stretching vibration and intermolecular H-bonded

Files

Steps to reproduce

show the highest peak at 3744 to 3373 cm-1, which means that there was a presence of Hydroxyl groups and there was O-H stretching vibration and intermolecular H-bonded