Fatigue test data for GLARE 2

Published: 5 July 2019| Version 1 | DOI: 10.17632/cr2gzjhmcx.1
Contributor:
Wei Sai

Description

Laminate layup: 1. Two layers of Al2024-T3 with four layers of 0-degree glass fiber prepreg (adhesive Redux 609 was applied between the aluminum and prepreg interface) 2. Two layers of Al2024-T3 with four layers of 90-degree glass fiber prepreg (adhesive Redux 609 was applied between the aluminum and prepreg interface)

Files

Categories

Fatigue Life

Licence