Battery Degradation Dataset - Li Plating And SEI Growth
Published: 6 August 2024| Version 1 | DOI: 10.17632/m8w8sjk3vm.1
Contributors:
Jiwei Yao, Qiang Gao, Tao Gao, Benben Jiang, Kody PowellDescription
45 commercial Li−ion coin cells (LIR2025H produced by EEMB Battery) with nickel manganese cobalt oxide (NMC) cathodes and graphite anodes are cycled on a Landt CT3001A battery test system to generate cycle data. The cells are charged under CCCV profile with constant current range from 0.2C to 5.5C. The cutoff voltage ranges from 4.2V to 4.4V. All cells are discharged with C/5. The detail charging profile can be found in the charging policy.xlsx. If you make use of our data, please cite our dataset directly using its DOI.
Files
Institutions
- University of Utah
- Tsinghua University
Categories
Aging, Lithium Battery