How a Zn Interlayer Modifies the Corrosion Failure Mode of Al/Steel Friction Stir Welds
Description
Dissimilar Q235 steel and 6061-T6 Al alloy were joined by friction stir welding (FSW) at 400, 550, and 700 rpm, with and without a Zn interlayer. Weld quality and mechanical properties led to the selection of 550 rpm. At this speed, the Zn interlayer increased the yield strength from 72.9 to 120 MPa and the tensile strength from 140 to 166 MPa. This is attributed to refinement of the continuous interfacial Fe–Al intermetallic compound (IMC) layer into an undulating, interlocking morphology. The corrosion behaviour of the joints was evaluated by potentiodynamic polarisation and scanning vibrating electrode technique (SVET) in 3.5 wt.% NaCl at pH 5, 7 and 9. With the Zn interlayer, icorr decreased at pH 7 but increased at pH 5 and 9. SVET revealed that at pH 5, corrosion mode shifted from localised, crack-prone IMC dissolution to a diffuse pattern, mitigating interfacial cracking. At pH 7, local anodic and cathodic activity was homogenised, enhancing resistance to uniform and localised corrosion. At pH 9, the Zn-rich layer progressively passivated and acted as a sacrificial anode, protecting the Al substrate. These results demonstrate that the Zn interlayer altered the corrosion failure mode of the dissimilar joints rather than merely altering the overall corrosion rate.
Files
Institutions
- Guangdong University of TechnologyGuangdong, Guangzhou