Fatigue characterisation of DC01 low carbon steel

Published: 1 November 2026| Version 1 | DOI: 10.17632/pgm74mvtyp.1
Contributors:
,
,
,

Description

Experimental high-cycle fatigue dataset were obtained from DC01 low-carbon steel specimens subjected to resonant sinusoidal excitation using a uniaxial electrodynamic shaker. A total of 296 fatigue tests were conducted across eleven experimental campaigns, including eight staircase campaigns involving 262 specimens and three strain-life (ε-N) campaigns involving 34 specimens. The specimens were subjected to fully reversed bending near their first bending resonance frequency using Sine Resonance Track and Dwell (SRTD) testing. The dataset includes individual loading levels, fatigue lives, failure/runout outcomes, initial frequency-sweep measurements, and time histories of acceleration, strain amplitude and tracked excitation frequency. Fatigue life was determined in post-processing using a criterion corresponding to a 2% decrease in tracked excitation frequency. Eight additional tensile tests performed at different crosshead speeds provide complementary stress-strain curves for mechanical property characterisation. The dataset can support fatigue-strength characterization at a target life, benchmarking of statistical methods for fatigue-strength estimation, evaluation of staircase testing strategies and investigation of dynamic response evolution during two control strategies

Files

Steps to reproduce

The fatigue tests were performed using the Sine Resonance Track and Dwell (SRTD) procedure, which consists of two successive stages. First, a sine sweep is performed over a predefined frequency range to identify the initial resonance frequency of each specimen. The resonance is identified from the maximum amplitude of the measured response and the associated phase variation in the vicinity of resonance. The frequency-sweep measurements are stored in text files and can be linked to the specimen-level dataset through the corresponding campaign and specimen identifiers. Once the initial resonance frequency has been identified, the excitation frequency is continuously adjusted to track changes in the specimen's resonance frequency during fatigue testing. This tracking procedure maintains the excitation near resonance as the dynamic behavior of the specimen evolves. Two control modes were used across the experimental campaigns: acceleration control, in which the excitation acceleration was maintained at a prescribed level, and strain control, in which the measured strain response was maintained at a prescribed level. Both acceleration and strain responses were monitored throughout the tests. As fatigue damage develops, the associated reduction in structural stiffness may lead to a decrease in resonance frequency. Since complete fracture is not necessarily reached during resonant fatigue testing, a 2% decrease in resonance frequency relative to its initial value was adopted as the experimental fatigue criterion.

Institutions

Categories

Mechanical Vibration, Fatigue Behavior

Licence